I shall be thankful if someone can give me the chemistry of this alloy. I hope I have got the alloy name correct.
Thanks in anticipation.
 
arunmrao,

check out this web site:

It is in German, but from what I understand, the chemistry is the following:
3C-0.7Si-0.5Mn-15.5Cr-0.5Ni-1.5Mo-other.

The spelling is actually G-X 300 CrMo 15 3, so if you do a research on you'll get the website mentioned above as well as some other useful links.

Good luck.

Coka
 
Thanks Coka. I did get to the site you mentioned,but I seemto have missed it. This was the easier way out to get a reply. Star to you.
 