I need some advise. We have a rust reworking process which uses a caustic solution (20% sodium hydroxide with water) to kill the rust. In our experience this works very well to kill the rust on tool and chrome type steels we put through this process.
However on one particular component, we have areas of the naked base steel (which show signs of rust), together with areas of silver plating. If I put this component through the caustic solution, and completely drain off all caustic solution and protect with rust protective oil, will the silver plating be ok?
I know that if the caustic solution is left on the component for some time it will attack the silver plating (green/brown discolorations). However if the caustic solution is completely removed, and drained off, with the silver plating not showing any form of chemical attack, and stored in rust preventive oil - Will the silver plating continue to deteriorate over time (eventually showing green/brown discolourations)?
My assumption is the silver plating will be ok, so long as the as the chemical source for the plating attack has been removed.
Thanks
Ian
I need some advise. We have a rust reworking process which uses a caustic solution (20% sodium hydroxide with water) to kill the rust. In our experience this works very well to kill the rust on tool and chrome type steels we put through this process.
However on one particular component, we have areas of the naked base steel (which show signs of rust), together with areas of silver plating. If I put this component through the caustic solution, and completely drain off all caustic solution and protect with rust protective oil, will the silver plating be ok?
I know that if the caustic solution is left on the component for some time it will attack the silver plating (green/brown discolorations). However if the caustic solution is completely removed, and drained off, with the silver plating not showing any form of chemical attack, and stored in rust preventive oil - Will the silver plating continue to deteriorate over time (eventually showing green/brown discolourations)?
My assumption is the silver plating will be ok, so long as the as the chemical source for the plating attack has been removed.
Thanks