Nov 8, 2023 #1 Laishetti Materials Joined Apr 19, 2023 Messages 17 Location IN Can anyone suggest which casting powder can be used for continuous casting (slab) of 17-4 PH stainless steel?
Can anyone suggest which casting powder can be used for continuous casting (slab) of 17-4 PH stainless steel?
Nov 8, 2023 #2 EdStainless Materials Joined May 20, 2004 Messages 16,399 Location Waukesha WI USA Why wouldn't you use what works for other SS grades? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
Why wouldn't you use what works for other SS grades? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Nov 9, 2023 Thread starter #3 Laishetti Materials Joined Apr 19, 2023 Messages 17 Location IN Is continuous casting of 17–4 PH possible or not? Upvote 0 Downvote
Nov 9, 2023 #4 3DDave Aerospace Joined May 23, 2013 Messages 11,544 Location US see https://www.eng-tips.com/viewthread.cfm?qid=186414 see https://www.carpentertechnology.com/alloy-finder/powderrange-17-4 see https://www.google.com/search?q="continuous+casting"+of+17–4+PH Upvote 0 Downvote
see https://www.eng-tips.com/viewthread.cfm?qid=186414 see https://www.carpentertechnology.com/alloy-finder/powderrange-17-4 see https://www.google.com/search?q="continuous+casting"+of+17–4+PH
Nov 9, 2023 #5 EdStainless Materials Joined May 20, 2004 Messages 16,399 Location Waukesha WI USA I know of multiple mills doing it. So possible, yes. Is it any better than slab cast? I am not sure about that. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
I know of multiple mills doing it. So possible, yes. Is it any better than slab cast? I am not sure about that. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed