In addition to the info from Meteng, there is some concern with room temp ductility for P92, and this would be worsened for a cast form.
From P J Ennis "creep strengthening mechanisms in 9-12% chromium steels" 2004,regarding P92 after exposure to service temps above 600C, "Although not seeming to have a detrimental effect on creep rupture strength ( indeed W additions are beneficial for the long term strength) the rather large Laves phase particles are responsible for a loss of room temperature ductility and impact strength"