Does anybody know of a spec for a cast equivalent for ASTM A276 S44004 steel (440C)?

Thanks

Bruv



 
I could not find any standard that included a high-carbon martensitic grade like 440C. ASTM A 217 covers martensitic stainless grades, but it is limited to carbon content of ~ 0.20-0.30, I believe. DIN 17445 likewise did not have anything close.
 