Nov 4, 2012 1 #3 patprimmer New member Nov 1, 2002 13,816 How long is a piece of string. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
How long is a piece of string. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules
Nov 6, 2012 Thread starter #5 dicer Automotive Feb 15, 2007 700 How detrimental is 700 deg F to grey cast iron, will it stress relieve enough to need remachining? I know remachining is needed if its into the 1400 deg F range. Sorry I ran out of time and just couldn't finish the first post. Upvote 0 Downvote
How detrimental is 700 deg F to grey cast iron, will it stress relieve enough to need remachining? I know remachining is needed if its into the 1400 deg F range. Sorry I ran out of time and just couldn't finish the first post.
Nov 6, 2012 #6 patprimmer New member Nov 1, 2002 13,816 It will only stress relieve at any temperature if it has frozen in stress to be relieved. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
It will only stress relieve at any temperature if it has frozen in stress to be relieved. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules
Nov 6, 2012 #7 M MintJulep Mechanical Jun 12, 2003 10,152 What grade of cast iron? What is the starting state of the piece? As-cast, machined, already tempered or annealed? Heated how? Cooled how and for how long? The possibility for distortion is largely dependent on geometry. Upvote 0 Downvote
What grade of cast iron? What is the starting state of the piece? As-cast, machined, already tempered or annealed? Heated how? Cooled how and for how long? The possibility for distortion is largely dependent on geometry.
Nov 6, 2012 Thread starter #8 dicer Automotive Feb 15, 2007 700 Just typical engine blocks heads etc. Upvote 0 Downvote