At what temperature will cast iron distort?
 
How detrimental is 700 deg F to grey cast iron, will it stress relieve enough to need remachining? I know remachining is needed if its into the 1400 deg F range. Sorry I ran out of time and just couldn't finish the first post.
 
It will only stress relieve at any temperature if it has frozen in stress to be relieved.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
What grade of cast iron?

What is the starting state of the piece? As-cast, machined, already tempered or annealed?

Heated how?

Cooled how and for how long?

The possibility for distortion is largely dependent on geometry.

 
Just typical engine blocks heads etc.
 