Nov 4, 2012 #1 dicer Automotive Joined Feb 15, 2007 Messages 700 Location US At what temperature will cast iron distort?
Nov 4, 2012 3 #2 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,258 Location JP All of them.[tt][/tt] Upvote 0 Downvote
Nov 4, 2012 1 #3 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US How long is a piece of string. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
How long is a piece of string. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules
Nov 5, 2012 #4 micalbrch Mechanical Joined Jan 9, 2010 Messages 955 Location DE 700 °C Upvote 0 Downvote
Nov 6, 2012 Thread starter #5 dicer Automotive Joined Feb 15, 2007 Messages 700 Location US How detrimental is 700 deg F to grey cast iron, will it stress relieve enough to need remachining? I know remachining is needed if its into the 1400 deg F range. Sorry I ran out of time and just couldn't finish the first post. Upvote 0 Downvote
How detrimental is 700 deg F to grey cast iron, will it stress relieve enough to need remachining? I know remachining is needed if its into the 1400 deg F range. Sorry I ran out of time and just couldn't finish the first post.
Nov 6, 2012 #6 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US It will only stress relieve at any temperature if it has frozen in stress to be relieved. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules Upvote 0 Downvote
It will only stress relieve at any temperature if it has frozen in stress to be relieved. Regards Pat See FAQ731-376 for tips on use of eng-tips by professional engineers & http://eng-tips.com/market.cfmfor site rules
Nov 6, 2012 #7 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,258 Location JP What grade of cast iron? What is the starting state of the piece? As-cast, machined, already tempered or annealed? Heated how? Cooled how and for how long? The possibility for distortion is largely dependent on geometry. Upvote 0 Downvote
What grade of cast iron? What is the starting state of the piece? As-cast, machined, already tempered or annealed? Heated how? Cooled how and for how long? The possibility for distortion is largely dependent on geometry.
Nov 6, 2012 Thread starter #8 dicer Automotive Joined Feb 15, 2007 Messages 700 Location US Just typical engine blocks heads etc. Upvote 0 Downvote