Hi All,
I'm trying to find out if I can hydrostatically pressure an ANSI 300 lb (PN50) flange, past it's pressure rating of PN50?
I have a stainless steel pipe with ANSI 300lb flanges on it. The operating conditions below 50 bar, however I need to undertake a hydrostatic pressure test (with water) approximately 20% above 50 bar.
Does any one know what the test pressure of these flanges and/or if there are any links/references that indicate what I can test the flanges to?