i have a customer that is an api 6a services shop
They had a wps and pqr made up but was written to aws d1.1 but the requirements need to be API 6A and NACE.If all requirements are meet can this procedure be used? The only problem i see with it is there was no charpys performed and from what i was reading charpys testing needs to be done in the weld and HAZ and satisfy the Base metal requirements which is 4130.Any help would be greatly appreciated.
They had a wps and pqr made up but was written to aws d1.1 but the requirements need to be API 6A and NACE.If all requirements are meet can this procedure be used? The only problem i see with it is there was no charpys performed and from what i was reading charpys testing needs to be done in the weld and HAZ and satisfy the Base metal requirements which is 4130.Any help would be greatly appreciated.