Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

C1035 Carbon Steel

Status
Not open for further replies.

Bagman2524

Structural
Jul 14, 2005
707
Is AISI 1035 Carbon Steel basically equivalent to A36? Is there such a thing as C1035 carbon steel. I assume it's AISI 1035.
 
Replies continue below

Recommended for you

1035 carbon steel is not equivalent to ASTM A 36 structural steel. The reason is that the carbon content for A36 structural steel is normally below 0.35% carbon content by mass for weldability.
 
any problem with using the 1035 as anchor bolt material?
 
Yes, what strength level do you need? Review ASTM A 325 or ASTM A 490 for bolt material composition and strength requirements.
 
Anchor bolts are normally equivalent to ASTM A-36, not high strength structural bolting.
 
Yes, correct, stanweld, I was thinking of structural bolting connections.
 
1035 is not typically used for anchor bolts, because specifications like ASTM A307 and F1554 require the carbon content to be < 0.26% for small sizes, < 0.29% for large. The limitation is for weldability, so if your application does not require weldability, then 1035 may be an acceptable alternative.
 
Bagman,

If you want anchor bolt material, then you should order to the anchor bolt spec F1554 to the strength you specify. Fasteners are serious business and one should not try to use material not certified to conform to the appropriate specs. This is particularly important with anchor bolts, where failures can result in injury. Also, note that the AISI/SAE alloys (1035)only account for chemical composition, and not for structural properties. Note that F1554 has additional requirements if weldability is required including tighter chemistries and carbon equivalency requirements.