Can anyone tell me the material of choice for bolting dual laminate (teflon/fiberglass) pipe flanges both flange to flange pipe and flange to steel(glass lined) vessel nozzle. Operating conditions are 100 psig, @ ambient, outdoors exposed to weather, pumping 100% bromine in the line. Currently using and ASTM 193 B7 but expeiencing rapid corrosion due to permeation of Br throught the teflon gasket.
 
It should be appropriate to use Teflon gasket and bolt material of ASTM 193 B7.

Timothy C. Odom, CEO
Odom Industries, LLC
Phone: 513-777-3773
Fax: 513-777-7223
 
Thanks Tim, that is the bolt we are using, however without the gasket.
 
Have you tried Xylan coated A193-B7 bolts? Xylan is a very thin PTFE based coating than only increases the fastener pricing slightly. It is used a lot in general chemical industry environments. I cannot comment on specific experience with bromine.
 
We haven't tried it but considered it. We had some concern that because the bromine readily permeates the teflon and may mask a corrosion problem. Since the PTFE is thin it may not be a problem and may be worth a shot. How about the effect on torgue? Any idea regarding changes we currently torque bare unlubed to 25 ft-lbs?
 
ElderX,

Coated carbon steel bolts may not work for you. The coating may not stop the Br, and it can be abraded during assembly leaving no protection. I would recommend using more resistant material such as stainless steel or titanium. I have no direct experience with Br, so I will assume it behaves similarly to Cl. Titanium alloys are nearly impervious to Cl corrosion, so I would consider them first.

If you do choose to coat the existing bolts, then you need to change the torque based upon the friction coefficient. The preload developed from a given input torque is directly proportional to friction coefficient. I would estimate the bare friction coefficient at 0.20-0.25, and PTFE would be around 0.10. Therefore, you should use about 1/2 the original torque. If this is a critical application, I would perform testing to confirm the friction coefficient levels.

Cory
cpadfield@omnimetalslab.com
 
Hi ElderX,

Why don't you try for sleeved bolting like one does for insulating flanges in the Pipelines, this may prevent a direct exposure with Br.