Hi, I have two questions. First off what grades are A307, A325, and A490 bolts? Second what is the formula to convert kips to foot pounds? I appreciate your time and information. Thanks, Cory
 
Replies continue below

Recommended for you

Working with US units can be quite confusing if you haven't been brough up with them, which includes just about everyone outside the US and Liberia! Here are a few key conversion factors.

Mass/Length
1 lb/ft = 1.488 kg/m
1 lb/yd = 0.4961 kg/m

Mass/Area
1 lb/ft2 = 4.882 kg/m2

Force
1 kip = 4.448 kN

Moment
1 kip-in = 0.113 kNm

Stress
1 kip/in2 = 6.895 MPa

Modulus
1 in3 = 16387 mm3

Second Moment of Area
1 in4 = 416231 mm4
 
A307 is basic carbon steel with an allowable tensile stress of 20 ksi.
A325 is a high strength heavy hex structural bolt with an allowable tensile stress of 44 ksi and has 3 different types (Type 1, Type 2 and Type 3).
A490 is a heat treated heavy hex structural bolt with an allowable tensile stress of 54 ksi.
 