Can anyone think of a reason one should be failing bend tests but passing pull-off adhesion tests?
Also, I wonder if we're failing or just doing the test wrong. The obvious fails look just like the failing picture in SSPC CS-23 or AWS C2.18. But the rest look just like the "marginal" picture, except that a sharp knife will pick off the coatings at every crack location. Does "lifting" mean doesn't take much with the knife to knock it loose, or we can pick it off in any way? Does "knife" mean dull putty knife, or sharp utility blade?
Hg
Eng-Tips policies: faq731-376
Also, I wonder if we're failing or just doing the test wrong. The obvious fails look just like the failing picture in SSPC CS-23 or AWS C2.18. But the rest look just like the "marginal" picture, except that a sharp knife will pick off the coatings at every crack location. Does "lifting" mean doesn't take much with the knife to knock it loose, or we can pick it off in any way? Does "knife" mean dull putty knife, or sharp utility blade?