I have a 1" or 1 1/2" C1045 shaft extending into a 375 deg F enviroment. The shaft rotates at 700-900 RPM.
Question is what do I use for a bearing?
 
Forgot to add, the shaft should be contained to .010" of movement when the shaft is cold (room temp.)
 
The best method I suggest is talk to the Bearing people because this is a highly researched area,Timkin, SKF, INA, FAG etc, who may have a bearing for this temp. (which is not very high). The most important part is that lubrication is available at all time and adequate internal bearing clearances. I would also size the bearing so that it is lightly loaded compared with its allowable dynamic rating.
We use such bearings with water cooling sleeves because or temepratures are much higher.
 
Thanks dooron:
The water cooling is worth looking at, heat treatment stabilisation bearing peek out at 125 deg. C which is a little short of 190C/375F but the water cooling my keep it down. Iam not sure what the heat conduction through the shaft will be if the bearing is within 3"-4" of the heat sorce.
 
Geomar,
Not sure how clean of a process you have, but if you can stand some bearing dust over time, look at Graphalloy Corporations bearings ( They are meant for high temp environements if you can stand a sleeve bearing for your application. They can be impregnated with a variety of metals to enhance performance. Also, from what you are telling me temperature wise, I wouldn't be surprised if you could use an off-the-shelf bearing for you application with the proper grease and lube frequency. The temps you are reporting are not all that high. As mentioned in another post, check with your bearing rep or better yet, try to get a tech guy inside the factory...
 