carnahanad
Structural
Some beam web openings were cut larger than what I had called out on plan for a project. The beams are W12x14; pretty small. The current size violates the detailing and geometric requirements of the design guide so I need to "fix" the beam.
I’m looking for a little guidance on what to do:
1. First thought is to have them fab new beams with the correct size as they aren’t matching the construction documents.
2. Sandwich plates on either side to essentially add web back into the beam, a little worried about the force transfer and the discontinuous web.
3. Add a single plate, cut to required shape that would fill in the web. The web is only 3/16” so this wouldn’t be too much work.
Just curious if anyone else has run into this.
I’m looking for a little guidance on what to do:
1. First thought is to have them fab new beams with the correct size as they aren’t matching the construction documents.
2. Sandwich plates on either side to essentially add web back into the beam, a little worried about the force transfer and the discontinuous web.
3. Add a single plate, cut to required shape that would fill in the web. The web is only 3/16” so this wouldn’t be too much work.