Hi all,
I'm developing wall thickness calculation for 18" ASTM A 928 UNS S32750 pipe, but I can't find basic allowable stress for this material in ASME B31.3. Is it possible to use the ASTM A 790 basic allowable stress value for A 928? Please kindly advise.
Regards.
I'm developing wall thickness calculation for 18" ASTM A 928 UNS S32750 pipe, but I can't find basic allowable stress for this material in ASME B31.3. Is it possible to use the ASTM A 790 basic allowable stress value for A 928? Please kindly advise.