Hello all,
We have a corrosion problem with the baseplates of a horizontal pressure vessel (ASME stamp) and we need to replace those baseplates. I have the follow question: Is this work a REPAIR according NBIC?

NOte:This work will not affect any pressure retaining element.

Thanks for your comments.
 
Replies continue below

Recommended for you

No, this would not require an NBIC Repair in my opinion as the baseplates and other non-pressure components are not under the purview of the ASME code, but if you wanted to you can probably find a contractor that will stamp the vessel and prepare an R-1 form.