Interpretation: IX-89-100
Subject:
Date Issued: January 2, 1991
Section IX, QW-202'2 and QW-451
File: BC90-663
Question: A procedure qualification in a test coupon of 1-1/2 in. thickness has been qualified
to the requirements of QW-202.2(a) with the exception of notch toughness. A second Procedure
Qualification with identical essential and siipplementary essential variables, is tested for notch toughness
only, in a test coupon of 3/16 in. thickness. Do the above two Procedure Qualifications support
a WPS to weld a butt joint 3/16 in. to 8 in. in thickness where notch toughness in required?
Reply: Yes

My question is that why dont the base metal qualification range starts from 3/32 to 8 inch? when impact test is required?
 
It may, but the inquirer did not ask that question.
 
Expecting some more insights
 
You may need to ask that question yourself. Submit an official inquiry.
 

Interpretation: IX-89-100
Subject:
Date Issued: January 2, 1991
Section IX, QW-202'2 and QW-451
File: BC90-663
Question: A procedure qualification in a test coupon of 1-1/2 in. thickness has been qualified
to the requirements of QW-202.2(a) with the exception of notch toughness. A second Procedure
Qualification with identical essential and siipplementary essential variables, is tested for notch toughness
only, in a test coupon of 3/16 in. thickness. Do the above two Procedure Qualifications support
a WPS to weld a butt joint 3/16 in. to 8 in. in thickness where notch toughness in required?
Reply: Yes.


Same case as above is this the lower limit is 3/32?
 
Why would you expect it to be 3/32"? You have only shown that impacts are good to 3/32"...not tensiles or bends.
 
For thickness less than 6mm the qualified minimum thickness is T/2? Am i right (when impact test is required) so the minimum thickness that wps is qualified is from 3/32 am i right? That means the above two procedures Combine a thickness range of 3/32 to 8"?
 
No. You haven't done any tension or bends to show the weld is sound for less than 3/16". You have only proven that impacts are good to 3/32".
 
Thanks david thats a clear shot.
 
I'm not sure whether the T/2 when T< 1/4" was valid back in 1989. Regardless, david is correct.
 