Interpretation: IX-89-100
Subject:
Date Issued: January 2, 1991
Section IX, QW-202'2 and QW-451
File: BC90-663
Question: A procedure qualification in a test coupon of 1-1/2 in. thickness has been qualified
to the requirements of QW-202.2(a) with the exception of notch toughness. A second Procedure
Qualification with identical essential and siipplementary essential variables, is tested for notch toughness
only, in a test coupon of 3/16 in. thickness. Do the above two Procedure Qualifications support
a WPS to weld a butt joint 3/16 in. to 8 in. in thickness where notch toughness in required?
Reply: Yes
My question is that why dont the base metal qualification range starts from 3/32 to 8 inch? when impact test is required?
Subject:
Date Issued: January 2, 1991
Section IX, QW-202'2 and QW-451
File: BC90-663
Question: A procedure qualification in a test coupon of 1-1/2 in. thickness has been qualified
to the requirements of QW-202.2(a) with the exception of notch toughness. A second Procedure
Qualification with identical essential and siipplementary essential variables, is tested for notch toughness
only, in a test coupon of 3/16 in. thickness. Do the above two Procedure Qualifications support
a WPS to weld a butt joint 3/16 in. to 8 in. in thickness where notch toughness in required?
Reply: Yes
My question is that why dont the base metal qualification range starts from 3/32 to 8 inch? when impact test is required?