Hi,
I can weld the B729 N08020 with the filler metal ENiCrMo-3?
In the analysis of the chemical composition which composition must be taken into consideration, that of the filler metal or the base material?
Thank you all.
Emilio A.
 
Yes. It is often done. You may also use E/ER320LR.
 
Hello weldstan,
Thanks for your cooperation.
If I welding the B729 N08020 with the filler metal ENiCrMo-3, which chemical composition can I expect when I do the PMI (Positive Material Identification)?
The Code Project is ASME B31.3.

Grazie,
Emilio A.
 
Closer to the ENiCrMo-3, but not the same depending on dilution which will be a factor of thickness of materials welded, joint design and welding heat input.
 
Thank you...
So for example the following composition in weld areas may be acceptable:

Cr = 19.490
Ni = 43.570
Mo = 6.828
Nb = 2.411
Fe = 23.500

There is a reference in the Code governing these limits?

Thanks,
Emilio A.
 
It could be. There is no Code requirement for the weld metal analysis other than successful qualification of the WPS with an F43 filler metal.
 