Article 344.5.2 specifies 100% radiography for girth and miter groove welds in paragraph (a) and random radiography for the same welds in paragraph (b). How do I discriminate between the two rules?

We have a pipe to pipe butt weld 55mm thick.
(We do not have a fabricated branch connection)
 
I think that you may be confused. The extent of examination is defined in Section 341.4. Section 344.5.2 provides for which type of welds RT is applicable.

 
Thanks for your comment, but my confusion is really in the fact that girth and miter groove welds are both specified in paragraph 344.5.2 as 100%RT in (a) and random in (b).
 
The rules in 344.5.2(a) apply to those miter and girth welds in pipe systems subject to 100% examination per 341.4.3.
The rules in 344.5.2(b) apply to those miter and girth welds in pipe systems subject to random examination under 341.4.1(b) and M341.4(b).

 