I have read a closed thread on this topic from 2010 with minimal success. I am looking for information on where I can purchase AWS/ASME A5.9 ER309LMo.
Houston office Kobelco, TG-S309MoL claimed they did not make it even though it is in their catalog
Metrode is close, just not the same classification.
Exocor is not certified only deemed "similar"
Special Metals, ESAB, Techalloy, Midalloy ect. are all made to the EN ISO standard
Any help on finding this wire or explanation on the discontinuation of AWS/ASME classification would be appreciated.
Thank you.