Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for AWS equivalent weld procedure and filler material to DIN procedures

Status
Not open for further replies.

AlbertaMecchie

Mechanical
Joined
Feb 17, 2021
Messages
20
Location
CA
Hi, I am working on a project, where lugs will be welded to structural carbon steel plate.
The lug supplier lists the following DIN standards for welding lugs to mild or low alloy steel, is there an AWS equivalent or near equivalent for procedure / filler materials ?
DIN EN ISO 2560-A: E 42 6 B 3 2 H10
DIN EN ISO 2560-A: E 38 2 B 1 2 H10

Thanks !
 
7016 or 7018
These are standard, basic rods with relatively low hydrogen requirements.
 