I have to help client put a WPS together for lap splice of # 11 bar , looking @ para. 3.6 "Lap Joints" reqs. dbl flare V groove welds (fig 3.4 (A) , except that a single flare V groove may be used if accessible from one side only , and approved by Eng.
Para . 3.6.2 also show a indirect lap splice with a splice plate,
My ? I don't see a fig. associated with the single flare V groove option , as we'er faced with that issue.it would seem to me that the single flare V groove weld option would req. a larger flare weld but maybe not
Para . 3.6.2 also show a indirect lap splice with a splice plate,
My ? I don't see a fig. associated with the single flare V groove option , as we'er faced with that issue.it would seem to me that the single flare V groove weld option would req. a larger flare weld but maybe not