ASTMA 487 GR 4QM and T24S

Status
Not open for further replies.

mikeweld

Mechanical
Joined
Jan 7, 2005
Messages
2
Location
US
Are the above grades of stainless steel suitable for use in an H2S environment.

Thanking you in anticipation.
 
ASTM A-487 grade 4QM and A-487 grade T24S do not exist. Grade 4Q (old designation) is not a stainless steel. It is a nickel-chrome-moly low alloy steel with less than 1% Nickel.

 