Jan 7, 2005 #1 mikeweld Mechanical Joined Jan 7, 2005 Messages 2 Location US Are the above grades of stainless steel suitable for use in an H2S environment. Thanking you in anticipation.
Are the above grades of stainless steel suitable for use in an H2S environment. Thanking you in anticipation.
Jan 10, 2005 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US ASTM A-487 grade 4QM and A-487 grade T24S do not exist. Grade 4Q (old designation) is not a stainless steel. It is a nickel-chrome-moly low alloy steel with less than 1% Nickel. Upvote 0 Downvote
ASTM A-487 grade 4QM and A-487 grade T24S do not exist. Grade 4Q (old designation) is not a stainless steel. It is a nickel-chrome-moly low alloy steel with less than 1% Nickel.