I am in the process of performing rough engineering calculations for the design of a sump pump system.
The process fluid is 10% HCL with abbrasive particles of about 10% by weight , the system temperature is about 50 degrees celsius. I did a little research and arrived at the the conclusion that ASTM A518 Gr 2 had the most acceptable rates of corrosion for this type of environment. I would like to go one step further and suggest the type of material specification for the pump impeller, cartridge , casing , bearings for this type of servive . I would much appraciate if you could help me out here.
Cheers
I am in the process of performing rough engineering calculations for the design of a sump pump system.
The process fluid is 10% HCL with abbrasive particles of about 10% by weight , the system temperature is about 50 degrees celsius. I did a little research and arrived at the the conclusion that ASTM A518 Gr 2 had the most acceptable rates of corrosion for this type of environment. I would like to go one step further and suggest the type of material specification for the pump impeller, cartridge , casing , bearings for this type of servive . I would much appraciate if you could help me out here.
Cheers