I am developing a WPS (butt weld) for F22 material. I am looking for the PWHT information for this material, does anyone know where this may be located? (ASME VIII for instance)?
 
Replies continue below

Recommended for you

KimberleyS;
I would use the code of construction - piping (B31.x) or ASME Boiler and Pressure Vessel Code (Section I or VIII, Div 1). Section VIII, Div 1 is UCS-56.
 