Soln
Civil/Environmental
- Mar 9, 2010
- 79
I'm confused by the ASME IX, 403.2, "the max thickness qualified is the thickness of the coupon", and 403.6, "the minimum base metal is T/2 when T<1/4".. Compare that to the table 451.2, where a coupon over 3/8 is qualified for thickness range from 3/16 - 2T.
I want to develop a WPS that ranges from 1/8 - 2". I'm thinking of using a coupon <1/4, and a 1" coupon. Does that cover my range? Am I missing a coupon between 1/2" and 1" for that range thickness? Or, if we qualify the min and max does that cover us?
I want to develop a WPS that ranges from 1/8 - 2". I'm thinking of using a coupon <1/4, and a 1" coupon. Does that cover my range? Am I missing a coupon between 1/2" and 1" for that range thickness? Or, if we qualify the min and max does that cover us?