Jan 7, 2024 #1 nabeel3 Mechanical Joined Dec 14, 2006 Messages 146 Location SA Dear Experts, In ASME Sec IX QW 451.1 is for the Transverse bend test and 451.2 longitudinal bend test. How can we decide when I have a specimen of thickness "t" which bend test is to be performed?
Dear Experts, In ASME Sec IX QW 451.1 is for the Transverse bend test and 451.2 longitudinal bend test. How can we decide when I have a specimen of thickness "t" which bend test is to be performed?
Jan 8, 2024 #2 r6155 Mechanical Joined Jan 12, 2010 Messages 3,048 Location AR See QW-161.1 and .2 Regards Upvote 0 Downvote