The following welding is required:
1. BS1501-151 Gr.430A to SA-516 Gr.70
2. BS1501-151 Gr.430A to BS1501-151 Gr.430A
3. SA-516 Gr.70 to SA-516 Gr.70
The company that will do the welding say they only have a WPS/PQR available for (3.) and wish to know if they can use it for (1.) and (2.) as well. Our inspector on site informed me that he sees no issue with this, his reasoning being that BS1501-151 Gr.430A is similar to ASME II P1 Group 1 material and as the WPS/PQR covers SA-516 Gr.70 (P1 G2) it can cover BS1501-151 Gr.430A as well.
Is his reasoning correct?
1. BS1501-151 Gr.430A to SA-516 Gr.70
2. BS1501-151 Gr.430A to BS1501-151 Gr.430A
3. SA-516 Gr.70 to SA-516 Gr.70
The company that will do the welding say they only have a WPS/PQR available for (3.) and wish to know if they can use it for (1.) and (2.) as well. Our inspector on site informed me that he sees no issue with this, his reasoning being that BS1501-151 Gr.430A is similar to ASME II P1 Group 1 material and as the WPS/PQR covers SA-516 Gr.70 (P1 G2) it can cover BS1501-151 Gr.430A as well.
Is his reasoning correct?