stevebro15
Specifier/Regulator
Gents
Reference Chapter V - 328.2.2.f
Is it permissable to allow STT Root & FCAW when B31.3 applies? It seems that clause QW 328.2.2.f relating to fluid piping forbids this? Is this only applicable when using a PQR qualified by 'others' and not the manufacturer?
Reference Chapter IX - K328.2.1
There is no such clause restricting welding processes however it is not permissable to use PQR's qualified by others.
Is my understanding correct in that if the manufacturer qualifies the PQR it is permissable to use STT & FCAW?
Thanks in advance!!
Reference Chapter V - 328.2.2.f
Is it permissable to allow STT Root & FCAW when B31.3 applies? It seems that clause QW 328.2.2.f relating to fluid piping forbids this? Is this only applicable when using a PQR qualified by 'others' and not the manufacturer?
Reference Chapter IX - K328.2.1
There is no such clause restricting welding processes however it is not permissable to use PQR's qualified by others.
Is my understanding correct in that if the manufacturer qualifies the PQR it is permissable to use STT & FCAW?
Thanks in advance!!