Dear Friends
Process Piping - Carbon Steel Piping - 6" Sch XXS ( 21.9mm )- PWHT done on the same butt joint twice. RT done after 1st PWHT-It passed.Is it acceptable to ASME B31.3?
What harm done to the joint ( weld metal & HAZ ) undergone PWHT twice, in terms of Mechanical Properties.... etc.
Thanks
 
You didn't mention the material as you know CS covers a lot of materials.
If your material is A106 no harm done.

Please comeback with the piping specification for a more definitive answer..
 
The only issue should be if supplementary essential variables are being applied and QW-407.2 of ASME IX has to be invoked: the original PQR may not have achieved the requisite 80% of the total time at temperature.

Steve Jones
Materials & Corrosion Engineer
 
RT after PWHT is not required for carbon steel under B31.3. refer to 341.3.1 (a).

 
Rt may not be required AFTER pwht but it is still required if dictated by the code...yes?
 
I think i see what you mean now Stanweld...it is not required again...sorry...
 
Hi, Friends
MATERIAL - ASTM A106 / ASTM A53 x 6" x 21.95mm.
Pls explain "QW-407.8(b)a change of more than 10% in the no of PWHT heat cycle following the welding cyscle"

Thanks
 
Steve
I don't get your points. Pls explain Thanks
 
Dear Friends
Material - ASTM A106/A3
I've been going through ASME B31.3 Chapter VI- Try to confirm extent of MPI if any required beside RT/UT for Process Piping Butt Welds.
If MPI required, please advise respective section(s).

I've concluded RT as per ABS Rules.ABS Rules do not require MPI.
Thanks in advance.
 
4872,
For MPI, refer to 341.4.3(b) and 302.3.3 (for castings).


 