Hello,
For 25 NB category M service line with 70 bar pressure, whether welded pipe/ERW pipe can be used for this case as per b31.3?
I don't find any such restriction for not using welded pipe.
Contradictorily, ASME VIII Div do not allow ERW pipes for lethal fluids.
I am confused whether or not to use welded pipe, as the pressure is quite high as well?
GD_P
For 25 NB category M service line with 70 bar pressure, whether welded pipe/ERW pipe can be used for this case as per b31.3?
I don't find any such restriction for not using welded pipe.
Contradictorily, ASME VIII Div do not allow ERW pipes for lethal fluids.
I am confused whether or not to use welded pipe, as the pressure is quite high as well?
GD_P