This has been bothering me for some time, I have noticed there is no longer a maximum depth of incomplete penetration on girth welds per Table 341.3.2 Acceptance Criteria for Welds. I remember in the past it was 1mm maximum depth, now it only refers to the cumulative length.
Hypothetically, what if you have a 6mm (1/4") thick weld and have 3mm deep incomplete penetration? Apart from having a bad welder, would this be acceptable to the code assuming it's cumulative length is acceptable... or am I missing something?
Hypothetically, what if you have a 6mm (1/4") thick weld and have 3mm deep incomplete penetration? Apart from having a bad welder, would this be acceptable to the code assuming it's cumulative length is acceptable... or am I missing something?