Wasn't sure whether to post this here or on the ASME site, but, since it is a weld question here goes:
This relates to a B31.1 pipe joint for shop fabricated manifolds:
We have a qualified WPS for SMAW on A106 pipe(P-1)with removable backing ring. Now would like to do the root passes with GTAW. We have a seperate qualified GTAW weld procedure for groove butt welds which was qualified on ASTM A515 and A516 plate, and this is also listed as a P-1 in B31.1.
Is it permissable to use my A515 GTAW procedure for a root pass on the A106 Pipe and finish off with my SMAW procedure?
A Code reference would be helpful and thanks.
Tom
This relates to a B31.1 pipe joint for shop fabricated manifolds:
We have a qualified WPS for SMAW on A106 pipe(P-1)with removable backing ring. Now would like to do the root passes with GTAW. We have a seperate qualified GTAW weld procedure for groove butt welds which was qualified on ASTM A515 and A516 plate, and this is also listed as a P-1 in B31.1.
Is it permissable to use my A515 GTAW procedure for a root pass on the A106 Pipe and finish off with my SMAW procedure?
A Code reference would be helpful and thanks.
Tom