Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME 16.5-2013 has no Pressure-Temperature ratings table for A182 Gr. F60 (Duplex SS 2205 Forgings)

Status
Not open for further replies.

Meck91

Mechanical
Joined
Aug 26, 2009
Messages
33
Location
CA
Hello,

ASME B16.5-2013 has no Pressure-Temperature ratings table for A182 Gr.F60 (Duplex Stainless Steel 2205) forgings. For example Table II 2-2.8 includes working pressure for A182 Grades F44, F51, F53 & F55 but no information for A182 Gr. F60. If i have to use this flange, how i can calculate the working pressure. Also, if i have to order this flange, i can't even specify the ASME code B16.5 in flange description, since this grade is not in ASME B16.5.

Please advise.

Thanks,

Meck91
 
For 2205 DSS, use F51 flanges (UNS S31803, I think). 2205 is UNS S32205, which is readily available nowadays as dual certified 31803/32205. 2205 is even replaced by the 31803 grade, as it has a beter chemistry (31803 is the predecessor so to say)
 