Dec 7, 2014 #1 krishh07 Mechanical Joined Dec 7, 2014 Messages 16 Location IN as per ASME Sex IX,if PQR done with P1 Gr1 to same,is it qualified for P1G1 and P1G2?please clarify Kind Regards M.K.Sridhar
as per ASME Sex IX,if PQR done with P1 Gr1 to same,is it qualified for P1G1 and P1G2?please clarify Kind Regards M.K.Sridhar
Dec 7, 2014 2 #2 gtaw Structural Joined Feb 10, 2006 Messages 1,988 Location US Yes, if toughness is not a requirement of the construction code, i.e., Section I, Section VIII, B31.1, etc. No, if toughness testing is required per the construction code. Best regards - Al Upvote 0 Downvote