as per ASME Sex IX,if PQR done with P1 Gr1 to same,is it qualified for P1G1 and P1G2?please clarify

Kind Regards
M.K.Sridhar
 
Replies continue below

Recommended for you

Yes, if toughness is not a requirement of the construction code, i.e., Section I, Section VIII, B31.1, etc.

No, if toughness testing is required per the construction code.

Best regards - Al
 