Mar 29, 2006 #1 fakhmed Mechanical Joined Dec 24, 2002 Messages 15 Location TN Hello Every body, What are the equivalent ASTM materials to API5LX52 ? Thank you
Apr 21, 2006 #2 giorgiobello Mechanical Joined Jun 29, 2005 Messages 6 Location IT I am not sure but I think "ASTM A 139 Grade E" has same SMYS and SMTS of API 5L X52: SMYS = 52kpsi SMTS = 60kpsi Upvote 0 Downvote
I am not sure but I think "ASTM A 139 Grade E" has same SMYS and SMTS of API 5L X52: SMYS = 52kpsi SMTS = 60kpsi
Apr 21, 2006 #3 giorgiobello Mechanical Joined Jun 29, 2005 Messages 6 Location IT SMTS = 66kpsi (for both materials) my mistake sorry Upvote 0 Downvote