Howdy all,

I'm looking for the NAS spec sheets for NAS6303 Thru NAS 6320. I looked in the usual places. All I could find on the assistdocs website was the addoption notice saying the standard was adopted. Not very useful. Thanks for the help.

-Kirby

Kirby Wilkerson

Remember, first define the problem, then solve it.
 
Replies continue below

Recommended for you

I'll check with our document control. We have most of them but this one was missing, so maybe we have access to it but just don't have a paper copy in the binder.

Thanks,

-Kirby

Kirby Wilkerson

Remember, first define the problem, then solve it.
 
You could also check your university libraries and see if they have it and fax it to you.
 
I wish I had access to a University Library.

-Kirby

Kirby Wilkerson

Remember, first define the problem, then solve it.
 
What did you need from NAS6303 Thru NAS 6320 spec?
 
Thanks rerig.

boo1, I was hoping to get shear and tension strenghts to use. I can calculate it, but generally when i need this information I prefer to just pull it from a spec for consistancy.

Thanks to everyone for your help.

-Kirby

Kirby Wilkerson

Remember, first define the problem, then solve it.
 
I checked the specification and could only find;
MATERIAL: A286(UNS S66286)
HEAT TREAT: AMS-H-6875 OR AMS2759: 160 – 190 KSI Ftu
 