Dear,

Could you have any refernece for ASME stainless steel pipes about minimum thickness requirement for impact test.

One EPC asked us to do the impact test for 304L welded pipes with size 219*3.76 and 323*4.57.

I check the specification of Shell, Total and DNV, Norsok M630, it specified that the pipe thickness below 6mm is no need to do the impact test.
But I didnot fimd any this kind of information in ASME standard.
 
It depends on the design code. Is this for B31.3, VIII-1, or some other code?

Huub
 
2,5 mm
See SA 370

Regards
 
And in most cases 304 would be exempt from impact test.
What pipe spec are you working with?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
Dimensions of Charpy impact specimen (full size or subsize) are the same for all codes.

@ Deanlover
You should make minimal effort to search for data and understand it before asking for help.
Please note that we work FREE for you.

See ASME VIII- 1 UG-84, UHA-51

Regards
 
r6155 said:
2,5 mm
See SA 370

That is the answer to a different question.

All answers are found in the Code and depend on design parameters.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
(OP) mentions “thickness” twice and three times in numbers: 3,76 mm, 4,57 mm and 6 mm. Does not mention temperature.

In ASME VIII div 1 UHA-51 minimum thickness is not mentioned for austenitic chromium nickel SS (304L)
Then the thickness is the minimum thickness of Charpy impact test specimen: 2,5 mm
Charpy impact test is not required for thickness less than 2,5 mm

Regards
 
deanlover said:
But I didnot fimd any this kind of information in ASME standard.
There is no blanket exemption for thicknesses less than 6mm. There are many exemptions listed in the Code of Construction, be it B31.3, Sec. VIII Div. 1, etc....especially for stainless steel. One of which is that impact tests are not required when the maximum specimen you can achieve has a width along the notch of less than 2.5mm.
But exemotion below 6mm is not universal. High pressure piping per B31.3 for example may require impact testing of thin stainless material.


 