Thanks for the additional info on Xypex. I have already asked the contractor to provide examples of local successful applications, preferably installed by their sub. So far I have not received anything from them.
My comments on Rinker were not meant to reflect Rinker as a whole, as I think they generally do a decent job with "normal" products, but rather the local construction industry. If I were in Miami or Atlanta, I expect Rinker could produce SCC. But here things are....different. We get home builders winning $50 million dollar condo projects. The quality of the labor we see on a daily basis is poor at best, appalling at worst.
I was even at a local seminar hosted by Grace and Rinker, where the topic was SCC. The Rinker rep was not local, nor was the Grace Rep. After they gave their talk, where they said SCC was such a great product and currently available from Rinker. I asked them why then could the local supplier not provide it, let alone even hear of it? I really stumped them both in front of about 100 other local engineers and building officials. Even after this seminar, by about 6 months, Rinker still could not provide it locally.