I need tie down some wood-frame shearwalls to an existing slab. I found a program PDA-2, Powers Design Assist 2, which does an astounding job, but I can't believe the values. I also doubt my own values.
e.g.
I find that a 3/8" PowerStud 2 embedded 2" into 2500 psi cracked concrete, at 2.875" from an edge is good for 1400 lbs.
If you are familiar with PDA, please comment.
e.g.
I find that a 3/8" PowerStud 2 embedded 2" into 2500 psi cracked concrete, at 2.875" from an edge is good for 1400 lbs.