There are a number of methods used for analyzing the chemical composition of metals, including ICP (inductively Coupled Plasma) with AES (Atomic Emission Spectroscopy), OES (Optical Emission Spectroscopy) using Arc/Spark/Glow Discharge, XRF (X-Ray Fluorescence), etc. You can obtain more information on these methods by using the following link: