Hello! I need same help to setup cutting condition for 12mm mild steel on Amada X1 laser. Overall cut is ok, but is burn the hols and slots. It melts the material. What would you change in condition to fix this problem? We using the condition 1 to pirce then start with 2 and run on 6.

12mm_cutting_condition_setup_l28tqf.jpg
 
What size holes/slots are they? It would help to know the diameter or size.

Try this:

Power: 2000 Watts
Freq: 800
Duty: 70
Feed: 800
Gas : 0.8
 
how would you set up pierce condition(1) and start condition (2)?
 
Thanks for your help. We sorted it out. There are code missing oin add func (00000010)

Can you share also cutting condition for 12mm stineless steel?
 
Laserkatana what machine do you use?
 
Currently I use Mitsubishi Fiber Lasers (GX) but I have used several CO2 and Fibers from them.
 