Sorry if this has been discussed already but i couldn't find the thread anywhere. My company has had the FO-3015nt for 8 years and we were wondering if there's any real benefit to switching to an Eco set up. We have the EZ cut system and most of the material we cut is Galvaneal steel between .090 and .180 thickness and also .25 through .375 HRS.
we currently run the AMADA 71502035 head and cone. Any ways just thought this would be a good place to ask. Thanks a ton!