Feb 4, 2011 #1 dsjon10 Mechanical Joined Dec 29, 2010 Messages 12 Location US I have a recent machining job where I had specified Aluminum 6061 type optional on the print. The shop came back and asked if I could use jig plate aluminum. What is jig plate aluminum and how does it differ from 6061?
I have a recent machining job where I had specified Aluminum 6061 type optional on the print. The shop came back and asked if I could use jig plate aluminum. What is jig plate aluminum and how does it differ from 6061?
Feb 4, 2011 #2 mcgyvr Mechanical Joined Aug 8, 2006 Messages 1,457 Location US Jig plate is cast stressed relieved aluminum with great surface finish that can eliminate the need for extra machining. Upvote 0 Downvote
Jig plate is cast stressed relieved aluminum with great surface finish that can eliminate the need for extra machining.
Feb 4, 2011 Thread starter #3 dsjon10 Mechanical Joined Dec 29, 2010 Messages 12 Location US Properties are similar as far as strength and elongation? Upvote 0 Downvote
Feb 4, 2011 #4 CorBlimeyLimey Mechanical Joined Nov 5, 2003 Messages 15,292 Location CA Some properties listed here http://www.alro.com/DIVSteel/STEELGUIDE_ALUMPLATE6.HTM Upvote 0 Downvote
Feb 4, 2011 #5 CorBlimeyLimey Mechanical Joined Nov 5, 2003 Messages 15,292 Location CA See also http://www.matweb.com/search/DataSheet.aspx?MatGUID=2b752c0339034c4e9d1aeb8855c195e9&ckck=1 Upvote 0 Downvote
Feb 4, 2011 #6 drawoh Mechanical Joined Oct 1, 2002 Messages 8,972 Location CA dsjon10, Some tooling (jig?) plate is magnesium. Make sure they are clear on what their material is. JHG Upvote 0 Downvote
dsjon10, Some tooling (jig?) plate is magnesium. Make sure they are clear on what their material is. JHG
Feb 4, 2011 #7 JMarv Mechanical Joined Jul 26, 2007 Messages 188 Location US Some more info on properties. http://www.clintonaluminum.com/pdf/8-12/K100_e-file.pdf Joe SW Office 2008 SP5.0 P4 3.0Ghz 3GB ATI FireGL X1 Upvote 0 Downvote
Some more info on properties. http://www.clintonaluminum.com/pdf/8-12/K100_e-file.pdf Joe SW Office 2008 SP5.0 P4 3.0Ghz 3GB ATI FireGL X1