I am looking for some help with the use of Aluminium Bronze valve discs in Chlorinated Swimming pool water. We are currently experiencing a build of Calcium on the valve disc. Not a corrosion issue just a build up of calcium on the valve disc. See attachment.
The values of the chlorine is 0.6ppm while, normal chlorine value for swimming pool water is 1.6ppm, tap water is normally 0 to 0.2 ppm.
Upstream the pumps and filters are stainless steel, with plastic piping.
The values of the chlorine is 0.6ppm while, normal chlorine value for swimming pool water is 1.6ppm, tap water is normally 0 to 0.2 ppm.
Upstream the pumps and filters are stainless steel, with plastic piping.